edmeister
Member
- Jun 25, 2002
- 97
Recently performed a weld repair to a solid 4130 1/2" dia shaft. My initial direction was to Weld / fill the chafe damage on the side of the shaft & perform a post-weld heat treatment to restore to original condition. It was brought to my attention that this was not an acceptable process. Say 10% of material diameter was compromised - best acceptance was 90% of shaft properties useful post weld repair. To regain the missing 10% - 4130 Sleeve is to be installed over top the filled in weld/blend & the sleeve welded at both ends. Is there any document / reference that does not allow original strength of a weld/repair? Any input would be interesting.