We are looking into rehabilitating piers of an abandoned rail bridge so that a pedestrian bridge can be installed.
There are no drawings available for the piers. There seems to be no reinforcement in the pier as concrete cover measuring device was not able to detect any rebar.
1. Can anyone please share drawings of a century old concrete rail bridge pier so we can learn how reinforcement was provided those days?
The project is only at brainstorming stage.
We are looking into rehabilitating piers of an abandoned rail bridge so that a pedestrian bridge can be installed.
There are no drawings available for the piers. There seems to be no reinforcement in the pier as concrete cover measuring device was not able to detect any rebar.
1. Can anyone please share drawings of a century old concrete rail bridge pier so we can learn how reinforcement was provided those days?