What's the relationship between cooling rate of melt and
undercooling ( Supercooling ) ??
does undercooling ( Supercooling ) increase when cooling rate of melt increases ??
If there 's no general rule in this subject, What's the relationship between cooling rate of melt and undercooling about pure aluminum ??
 
Replies continue below

Recommended for you

This is a pretty simple thought experiment, all you really need to do is consider why supercooling occurs....

Nick
 
Increase in cooling rate,will lead to an increase in undercooling.

" An introduction to solidification of metals" W. C. Winegard. The Institute of Metals: 1964


A beautiful publication , I lost my copy to someone and did not get it back.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
Thanks Maui . A star for you!!

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor