I'm reflowing pebax's over a PTFE liner with a mandrel inside. Having problems with particulate when removing the liner. Looks like the liner is being torn when pulling out the mandrel manually with a clamp (Requires a bit of force). The mandrel OD is 0.0005 smaller than the ID of the liner. Have tried 0.001 smaller as well but still getting the particulate problems. Currently trying to smoothen mandrel surface with 800 grit abrasive paper and trying to run at a lower reflow temp.
Any suggestions would be appreciated
JPC
Any suggestions would be appreciated