We kindly need advice regarding of
using fullsole to repair crack in joint weldment pipe 46 inch diam instead of repairing by cutting & rewelding?
Your cooperation in this regard will be highly appreciated.

Thank You
 
Replies continue below

Recommended for you

this reads like you copy/pasted an email you wrote that the welding engineer in your company ignored.

there's zero info here, dude
 
If you want to weld a plate over the crack a lot more information is needed
 
It may be fine if it’s a temporary repair for an existing equipment to prepare an O&M plan. It may not be preferred if it’s the weld defect on a new equipment.
 
Tarig
Not removing the crack, can cause more Cracks if just welded.
 