Huong83
Structural
- Sep 6, 2011
- 17
I currently review some structural drawings. Footing to be found on natural clay of 400KPa.
No soil class here. The slab on grade is 120 thick SL82 mesh. It look ok.
Strip footing typical is 300 wide x 600 deep (internal) and 450 wide x 600 deep (external double brick wall).
Residential strip footing are used with 300mm diameter mass bored piers at 2m max spacing. Bored piers are extended to hard clay foundation of minimum 450KPa foundation bearing stratum.
This 2 storey residential house (1st flor 200 thick reinforced concrete slab) is 11m wide 22m long.
Strip footing I think is enough to carry load ? so why use bored pier here and no reinforcement.
And the pier of 300mm diameter seem to be small to have enough soil bearing capacity ?
No soil class here. The slab on grade is 120 thick SL82 mesh. It look ok.
Strip footing typical is 300 wide x 600 deep (internal) and 450 wide x 600 deep (external double brick wall).
Residential strip footing are used with 300mm diameter mass bored piers at 2m max spacing. Bored piers are extended to hard clay foundation of minimum 450KPa foundation bearing stratum.
This 2 storey residential house (1st flor 200 thick reinforced concrete slab) is 11m wide 22m long.
Strip footing I think is enough to carry load ? so why use bored pier here and no reinforcement.
And the pier of 300mm diameter seem to be small to have enough soil bearing capacity ?