Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Retaining Wall Construction Joint Spacing 1

Status
Not open for further replies.

Boiler106

Structural
May 9, 2014
211
we've carried a 60ft maximum spacing for construction joints for concrete retaining walls for decades but we don't know where this originated. We've noted that many other firms carry this same requirement and we often get pushback from contractors.

from our research, we cant find anything concrete (ahem) on the subject.

does anyone know where this might have originated or where i can find some guidelines? CRSI retaining wall guide and ACI 224.3 do not seem to be of help.

It would seem to me that contraction joint spacing is far more critical and maybe construction joint spacing could be stretched.

thoughts?

 
Replies continue below

Recommended for you

I am not sure there is a definitive guide but there are lots of references.

Screenshot_-_Copy_xpiy5v.png


And here is something more in line with the spacing you gave.

Screenshot_-_Copy_onx9d6.png
 
It's either control the spacing of contraction joints or increase reinforcement to limit crack width. There is no need for construction joints if the contraction joints are done properly.
 