I need to add some window openings to an existing exterior 8" loadbearing CMU wall. Does anybody have some thoughts on how to best accomplish this? I can't add any structural reinforcement, concrete or steel, on the inside of the wall (no room). I have specified breaking out the face of vertical cells before, to add reinforcing, but I'm not sure how practical this is. As far as a header goes, I've heard of people sawing out the bed joint at the head of the opening, and inserting steel angles, but I've never seen a good detail.
Any thoughts would be appreciated.