Mowoki
Mechanical
- Jul 29, 2019
- 1
I am hearing and reading that ASTM A490 bolts and galvanized ASTM A325 bolts shall not be reused. I am also reading that although ASTM A490 bolts and SAE J429 grade 8 bolts are very similar in size and strength, but the head, thread length, and application are different.
It was strange to hear that ASTM A490 bolts cannot be reused as I thought going over yield is not desireable as it puts the hardware in danger of fatigue failure. Now, my question is if the SAE J429 grade 8 bolts also follow this rule. If we use the recommended torque range, my expectation is that the hardware will not be damaged, and thus may be reused. Am I missing anything?
It was strange to hear that ASTM A490 bolts cannot be reused as I thought going over yield is not desireable as it puts the hardware in danger of fatigue failure. Now, my question is if the SAE J429 grade 8 bolts also follow this rule. If we use the recommended torque range, my expectation is that the hardware will not be damaged, and thus may be reused. Am I missing anything?