I'm looking for heat treat temps and property data to see if these tool steels can withstand a 900 deg. F coating treatment without destroying their RC 65-67 hardness. Where or from whom can I find property data?

rayband

RAYBAND
Rock Island Arsenal
AMSTA-RIA-SEM
 
Replies continue below

Recommended for you

Unclelsyd,

Thanks for the fast response. Your comment and the links gave me all I needed.