Well, long story short. I have a situation where I'm supporting about 6" of soil from going underneath a continuous grade beam (washing underneath the grade beam) with rigid insulation. I just want to make sure it won't snap off.
I bet it will be quicker to get a piece and test it yourself than talk to the MFG. How long of a cont. piece is this? why is the footing being washed away?