Hajiwaji
Mechanical
- Jan 1, 2023
- 24
Dears,
I have wet sour crude line with about 30% water cut and over 100000 ppm of NaCl. The header is CS with internal FBE coating. For small bore piping smaller than 2" (branches, vents and drains) Alloy 625 is selected.
Is is possible to directly weld these dissimilar metals without risk of galvanic corrosion sense crude is not conductive? Or is it required to have an insulating gasket connection?
Thank you
I have wet sour crude line with about 30% water cut and over 100000 ppm of NaCl. The header is CS with internal FBE coating. For small bore piping smaller than 2" (branches, vents and drains) Alloy 625 is selected.
Is is possible to directly weld these dissimilar metals without risk of galvanic corrosion sense crude is not conductive? Or is it required to have an insulating gasket connection?
Thank you