Hello,
I'm José Isita, an engineer from Mexico. In the plant we have 2 RO Units, the first unit produces permeated water that we use in our product, and the second, treat the reject from the first unit for reusing it in other areas of the plant.
Since this water is softened and has lower conductivity, silica and minerals than our well water. I want to use it in the boilers of the plant. So I want to know if somebody has done that? And is you think that I will have savings on water, chemicals and diesel?
Here is some info about the situation:
Boiler Operating Pressure: 106 PSI
Steam Production: 10,000,000 lb/month
Well Water RO Water
Conductivity 850 400
Silica 80 50
Hardness 240 0
I'm José Isita, an engineer from Mexico. In the plant we have 2 RO Units, the first unit produces permeated water that we use in our product, and the second, treat the reject from the first unit for reusing it in other areas of the plant.
Since this water is softened and has lower conductivity, silica and minerals than our well water. I want to use it in the boilers of the plant. So I want to know if somebody has done that? And is you think that I will have savings on water, chemicals and diesel?
Here is some info about the situation:
Boiler Operating Pressure: 106 PSI
Steam Production: 10,000,000 lb/month
Well Water RO Water
Conductivity 850 400
Silica 80 50
Hardness 240 0