USER10
Materials
- Oct 12, 2007
- 17
Hello folks
i was checking if a road segment recently built can carry the loading of a temporary trailer (100000 pounds) without problems. The road is : Asphalt concert layer over granular base layer and sandy Subgrade materials both compacted to min of 95% Modified Proctor.
From the configuration of the trailer, i found that the worst loading scenario (highest surface pressure on the road) corresponds to a load of 50000 pounds over 2 foot by 2 foot concert pad, resulting in contact pressure of 100 psi.
My recommendation was( based on judgment) that the bearing capacity of the asphalt concert layer and the compacted granular base and sand subgarde underneath are likely much higher than the contact pressure of 100 psi. The settlement under such pressure should be small (less than 10 mm) and mostly elastic.
Just want to make sure that i did not miss anything . Any inputs please?
Thank you very much for your help
i was checking if a road segment recently built can carry the loading of a temporary trailer (100000 pounds) without problems. The road is : Asphalt concert layer over granular base layer and sandy Subgrade materials both compacted to min of 95% Modified Proctor.
From the configuration of the trailer, i found that the worst loading scenario (highest surface pressure on the road) corresponds to a load of 50000 pounds over 2 foot by 2 foot concert pad, resulting in contact pressure of 100 psi.
My recommendation was( based on judgment) that the bearing capacity of the asphalt concert layer and the compacted granular base and sand subgarde underneath are likely much higher than the contact pressure of 100 psi. The settlement under such pressure should be small (less than 10 mm) and mostly elastic.
Just want to make sure that i did not miss anything . Any inputs please?
Thank you very much for your help