Hi all, i have a following question.

Why root pass in welding of steels is preferred with E6010 though it has cellulose in its coating means it has moisture in its crystal lattice?

Thanx in advance
 
Replies continue below

Recommended for you

For carbon and low alloy steels the E6010 is a deep penetration rod.
 
It is also the fastest "freezing electrode on the market today. This allows the welder to have the greatest control over the weld puddle - a useful attribute when welding open roots

cheers,

stk
 