Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

rubber coating solution.

Status
Not open for further replies.

msc86

Chemical
Jan 9, 2013
6

Dear chemist , I want to ask you for an advice ,there is a possibility to restore rubber surfaces which have Been Scratched or pricked? There is a chemical solution (polymer , coating solution) that would fill these gaps?

Thanks you!
mihail
 
Replies continue below

Recommended for you


No, it is not natural rubber ,we talk about synthetic rubber.I'm looking for a coating solution.


 
Sir,
Those Scratched or pricked on rubber surface is "part after used in application or after molding?".
if it is after molding process then coating solution not work on surface.
if it is after application life then you can grind little bit surface (for roughness) then apply coating and the cure that coating,might work.
 


Hi all ,

Someone know what solution use this man in movie , thanks.


Link
 
Status