I have a few questions about cutting splines.
I'm not sure what splines these are... and what type of cutter to use...
I'm making a HD Rear Output shaft for my Dana 20 Transfercase... The only thing stopping me from finishing this project is the splines that go into the T-case and into a gear.... I counted the splines(15). I then measured the O.D. of the splines and Got 2.417".... With that I started plugging in numbers... This is what I figured...
Dp= 17/2.417= 7.0335" DP=7
ADD= 1/7= .1428"
CP= 3.1416/7= .4488"
CT= 1.5708/7= .2244"
CL= .15708/7= .02244"
DED= 1.15708/7= .1652"
WD= 2.15708/7= .30815"
PC= 15(.4488")= 6.732"
PD= 15(.1428")= 2.1428"
OD= 2.1428"+.2856"= 2.428"
RC= 1.812"
I have all of these numbers some probably N/A...If anybody knows what type of splines that a Dana 20 had and what cutter to use that would be great..
How would I know if these Splines are Involute, American Standard or Fellows Stub Tooth type?
Thanks.
I'm not sure what splines these are... and what type of cutter to use...
I'm making a HD Rear Output shaft for my Dana 20 Transfercase... The only thing stopping me from finishing this project is the splines that go into the T-case and into a gear.... I counted the splines(15). I then measured the O.D. of the splines and Got 2.417".... With that I started plugging in numbers... This is what I figured...
Dp= 17/2.417= 7.0335" DP=7
ADD= 1/7= .1428"
CP= 3.1416/7= .4488"
CT= 1.5708/7= .2244"
CL= .15708/7= .02244"
DED= 1.15708/7= .1652"
WD= 2.15708/7= .30815"
PC= 15(.4488")= 6.732"
PD= 15(.1428")= 2.1428"
OD= 2.1428"+.2856"= 2.428"
RC= 1.812"
I have all of these numbers some probably N/A...If anybody knows what type of splines that a Dana 20 had and what cutter to use that would be great..
How would I know if these Splines are Involute, American Standard or Fellows Stub Tooth type?
Thanks.