I noticed that on page A-7 of MMPDS-15, it is written that "S/N Curves are for a 50 percent probability of survival. We usually assume conservatively few fatigue penalization factors (such as anodizing + shot-peening, surface finish, ...). But, I would like to know if you apply another reduction factor on the S/N Curves of MMPDS to have a better confidence level? If you reduce these curve then please let me know what is your reduction factor? I appreciate if you can share your experience.
Thank you,
A.
I noticed that on page A-7 of MMPDS-15, it is written that "S/N Curves are for a 50 percent probability of survival. We usually assume conservatively few fatigue penalization factors (such as anodizing + shot-peening, surface finish, ...). But, I would like to know if you apply another reduction factor on the S/N Curves of MMPDS to have a better confidence level? If you reduce these curve then please let me know what is your reduction factor? I appreciate if you can share your experience.
Thank you,
A.