SA 350

Status
Not open for further replies.

GTDan

Mechanical
Sep 16, 2008
10
Good morning. Can you provide me with or point me in the right direction for the chemical composition of SA 350 lf2? I cannot find anything in ASME Section IX.

Thanks
 
Replies continue below

Recommended for you

GTDan;
ASME B&PV Code, Section IX provides guidance for weld procedure and welder qualification and does not provide chemical composition of code endorsed materials.

The chemical composition and mechanical properties for ASME SA 350 can be found in ASME B&PV Code, Section II, Part A ferrous material specifications or if you have access to an ASTM Specification, you can locate A 350.
 