good morning
i am trying to weld SA 517 grade B and S690 QL1 using SMAW electorde 11018 M for repair for transpot LPG pressure vessel but every time PQR fails at charpy v notch impact test give me max reading 26 joule
need for help please...
 
Replies continue below

Recommended for you

Plate S690 QL is for structural purpose, not for pressure vessels.

As I say in your post of 17feb20, you need a welding engineer.

Also contact a pressure vessel engineer.

Regards
 
i have pessure vessels head made from naxta 70 model 1980
that is why we decide to use it
 
This pressure vessel is very dangerous. I understand that you are not in a position to handle this issue.
Are you aware of your responsibility?