To what size specification is Schedule 160 Stainless Steel (316) pipe made? B36.19 (Stainless Steel Pipe) doesn't include Sch 160 but does state:
ASME B36.10M [wrought steel piping] includes other pipe thicknesses that are also
commercially available with stainless steel material.