Hi Folks,

I designed pipe columns that are supporting a steel beam but the contractor wants to use A316 stainless steel schedule 40 pipe columns. I could not find any values about schedule 40 pipe columns, and I designed columns for 3" dia. std. pipe column. Does anyone have any information or reference about the design values of Schedule 40 & 80 design values ?

Thank you for your time and energy!
 
Replies continue below

Recommended for you

Both the AISC and ASCE have design guides for stainless. Off Google. Not sure if there is a free download for the entire manual. You can get a few sections as I have done in the past. Bending allowable is less for stainless 304 than Steel(about 16.2KSI), so I would think it would be less for column buckling.
If your looking for a Column load chart for pipes, like in the AISC Steel manual, it may be in one of the above. If your looking for a approximate answer you could conservatively extrapalolate, and apply a reduction factor. If too close then I would get the above stainless codes.

The below will lead you too more refs


 
ASCI design guide 27, Structural Stainless Steel
I believe the doc number is 827-13

And two comments.
-SS will ave double the thermal expansion of CS. If this is where it can get hot and cold you might need to consider that.
-If the connection is exposed to the elements then you will need to isolate the connection to minimize galvanic corrosion of the CS.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Ya, definitely look at the design guides. Remember that SS has a somewhat nonlinear stress-strain curve, and this effects buckling the equations. So it's not just a matter of reducing allowable stress.
 
Good point SocklessJ I forgot to mention that. In the begining I used the values of AISC with a reduction factor till I saw that. It is better to use the stainless codes.
 