Hi to all,
my question is: a multiprocess PQR (GTAW+SMAW) can generate a WPS with only one of this process (for example only SMAW?)
I see QW 200.4 and I understand that is possibile can someboby confirm that?
 
Replies continue below

Recommended for you

Yes you can but you must remember you are governed by the weld deposit thickness of each process,
Regards,
DD
 
This is why in general I don't like the idea of combining multiple processes into a single PQR.