Hi to all,
my question is: a multiprocess PQR (GTAW+SMAW) can generate a WPS with only one of this process (for example only SMAW?)
I see QW 200.4 and I understand that is possibile can someboby confirm that?
 
Yes you can but you must remember you are governed by the weld deposit thickness of each process,
Regards,
DD
 
This is why in general I don't like the idea of combining multiple processes into a single PQR.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
 