Hello,
Anyone care to look at this failed shaft? - I'd like to know if it is fatigue or something else that might cause it to break like this?
I'm a little baffled because I can't see any beach marks or similar looking breaks from any books I have. It is 1045 material 1" diamter. It's load history is not known but is subject to bending and torsion.
Failure occured at a step down to 1" with a fairly tight radius and pretty heavy tooling marks...
I'll upload another picture in a bit
Thanks
Anyone care to look at this failed shaft? - I'd like to know if it is fatigue or something else that might cause it to break like this?
I'm a little baffled because I can't see any beach marks or similar looking breaks from any books I have. It is 1045 material 1" diamter. It's load history is not known but is subject to bending and torsion.
Failure occured at a step down to 1" with a fairly tight radius and pretty heavy tooling marks...
I'll upload another picture in a bit
Thanks