Hi All,
I was hoping to gain some insight on visible shear cracks in concrete beams. At what point does a visible shear crack become a concern? I've attached a picture of a crack in a parking structure beam; is this something to be concerned about?
Thanks for your input.
Bryan
I was hoping to gain some insight on visible shear cracks in concrete beams. At what point does a visible shear crack become a concern? I've attached a picture of a crack in a parking structure beam; is this something to be concerned about?
Thanks for your input.
Bryan