Anyone ever heard of an unpatterned nail popping in walls occurring in multiple locations in an old residence after new vinyl windows were installed?
I could attribute it to a humidity change, due to the new windows, possibly related to the type of nails used, but it seems a stretch.
Mike McCann, PE, SE (WA)
I could attribute it to a humidity change, due to the new windows, possibly related to the type of nails used, but it seems a stretch.