Hello,
I come to across a vessel which has 800 mm ID with 40 mm thk with Full RT.
Now due space constrain, Shell to dish joint is not possible with both side V groove weld (table-U-12-Type-1) & also due to project requirement, a backing strip is not permitted so table-U-12-Type-2 can not apply. So need to proceed with weld type table-U-12-Type-3 only. I have to ignore the limitations of this weld type which is acceptable?
With this configuration, can I consider the joint efficiency of shell 1 for long. seam & 0.6 for circumference seam?
Regards,
KPM
I come to across a vessel which has 800 mm ID with 40 mm thk with Full RT.
Now due space constrain, Shell to dish joint is not possible with both side V groove weld (table-U-12-Type-1) & also due to project requirement, a backing strip is not permitted so table-U-12-Type-2 can not apply. So need to proceed with weld type table-U-12-Type-3 only. I have to ignore the limitations of this weld type which is acceptable?
With this configuration, can I consider the joint efficiency of shell 1 for long. seam & 0.6 for circumference seam?
Regards,
KPM