masterx81
Automotive
- Dec 27, 2009
- 17
Hi!
I've done some work on the seat of an engine head, and now i can't find any shim that can i use for setting the valve clearances.
The clearance is set by a 11.5mm in diameter diameter shim that is placed just under the bucket, between the bucket and the valve stem.
The minimum shim that i can find is 2.00mm. I'd suppose that it's difficult to find shim under this value because this shims seem case hardened, and under 2.00mm the core can be too brittle, and can split in two under the load of the valve stem (6mm stem loading something like 60/70kg at max rpm, spring load + inertia).
I need some 0.95 /1.00mm shims, so i must find a way to machine them by my own.
I know that the tip of the valve is hardened at least at 53 hrc.
I've think about grinding the shims and get them nitrided, so that the core will be untouched.
Someone have a suggestion for me?
Really thanks!!!
I've done some work on the seat of an engine head, and now i can't find any shim that can i use for setting the valve clearances.
The clearance is set by a 11.5mm in diameter diameter shim that is placed just under the bucket, between the bucket and the valve stem.
The minimum shim that i can find is 2.00mm. I'd suppose that it's difficult to find shim under this value because this shims seem case hardened, and under 2.00mm the core can be too brittle, and can split in two under the load of the valve stem (6mm stem loading something like 60/70kg at max rpm, spring load + inertia).
I need some 0.95 /1.00mm shims, so i must find a way to machine them by my own.
I know that the tip of the valve is hardened at least at 53 hrc.
I've think about grinding the shims and get them nitrided, so that the core will be untouched.
Someone have a suggestion for me?
Really thanks!!!