there is a situation of a 15MW slip ring motor (uses liquid rotor starter) that has its slip ring shorting contacts sparking/ flashing - mostly when the motor trips from full load. On few occations they also spark during startup but this is not frequent. As a result the contacts need to be replaced now and again as they get badly damaged on the contact surface. This is a recent problem, the motors slip rings were replaced about 5 months ago as part of major overhaul. Can anyone suggests why this could be happening and what can be done to resolve this problem?