mattwilliamso2
Civil/Environmental
- Jan 16, 2010
- 3
I am looking to specify a shot blast finish for a new concrete pathway. We are specifying this to achieve the nice textured effect it produces. Could anyone help me with how to specify such a finish? I know we want a light shot blast finish but do not know what else I need to specify. Size of shot? Etc..
The concrete will be 5" thick slab on grade with a 2" polyfibre mixed in. Thanks for any help you can provide.
The concrete will be 5" thick slab on grade with a 2" polyfibre mixed in. Thanks for any help you can provide.