Recently, I’ve come across a finish treatment called ‘Shou Sugi Ban’. It was developed in Japan and consists of finishing exterior wood surfaces with a light ‘char’. This apparently provides a durable surface.

The improvements include making the surface more water resistand by closing open pores.

It also improves the insect and rot resistance. This includes improving the termite resistance.

It also improves the wood against external elements like sun and rain.

The charred surface apparently improves fire resistance. This latter item is surprising, since I was under the impression that prior char makes lumber more susceptible to fire damage.

Is anyone aware of this process and can anyone add additional information or confirmation of these enhancements.
 
Replies continue below

Recommended for you

I watch HGTV and YouTube all the time. There are a few videos using this technique. I have not tried it.
I once knew a guy that tried it and the wood popped. A pocket of sap inside the wood heated up and popped. So wear protection if trying it.
 
I'm aware of it - have a family member that had planned to use it as their siding, but never got around to the project. It was at its height of popularity around here 8 or 9 years ago. Don't hear much about it anymore, though it pops up every now and then. I seem to recall it being very expensive and difficult to source.
 
I've encountered it in the timber framing world - you may find some more information through the Timber Framers Guild.
 
If you dig into fire rating of heavy timber, the char layer develops and then provides protection for the remainder of the wood. So there's some credence to improving fire resistance by providing an intentional char layer on the materials.
 
If you dig into fire rating of heavy timber
I was aware of that... Mass timber can develop protection. I understand the char layer also makes the next exposure to fire easier even though it offers protection. The treatment is generally used for dimensioned lumber and cladding not mass timber.
 
Is there anyone that can verify the quality of the added advantages of using this process?
 
Anicdotally, here in Japan there are many old buildings (hundreds of years) with the charred finish still standing.

It was used extensively on "yagura", out buildings used to store valuable items.

My father in law's yagura has this finish, not sure how old it is.
 
The Japanese characters are 焼杉板.

Literally, burnt "sugi" plank.

Sugi is the Japanese ceder tree, which is anyways insect and water resistant.

Perhaps the heat polymerizes the natural ceder resins? Or maybe the benefits are basically those of the wood itself.

Your mileage may vary if applied to a different species of wood.
 
Thanks... if originally cedar, there are natural extractives that give it moisture, rot and insect resistance. Some cedars are better than others. Do you know if there are any tests undertaken to see if there's an improvement in the material?
 