Sep 24, 2002 #1 hanhee Materials Apr 10, 2002 4 0 0 KR I once used a silicon carbide fiber over 1 meter. Where to buy such fiber do you know?
Sep 25, 2002 1 #2 Padlofski Materials Dec 19, 2001 13 0 0 GB Performance Composites Ltd in the UK have various fibres left over from some MMC research projects including 'Nicalon' silicon carbide fibre Alumina fibre Boron filaments woven with titanium. P55 & P75 Carbon fibre. contact email sms@performance-composites.com Upvote 0 Downvote
Performance Composites Ltd in the UK have various fibres left over from some MMC research projects including 'Nicalon' silicon carbide fibre Alumina fibre Boron filaments woven with titanium. P55 & P75 Carbon fibre. contact email sms@performance-composites.com
Sep 25, 2002 1 #3 CoryPad Materials Apr 15, 2002 5,192 0 0 US A good producer of SiC fibers is Specialty Materials, Inc. - here is there site: http://www.specmaterials.com Upvote 0 Downvote
A good producer of SiC fibers is Specialty Materials, Inc. - here is there site: http://www.specmaterials.com