Tw, Please describe the meaning of this in asme b31.3. Thanks for your help

Thanks,
Tommy
 
Replies continue below

Recommended for you

It's defined on page 269 of the standard. Do you not have a copy?
 
Tommy3021,

It is the minimum wall thickness (nominal)of the components joined by butt weld.



Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
 
Generally speaking min and nom cannot be used interchangeably.

Regards,

Mike
 
Thanks to you all. EngeryMix your answer helped too.