How do I use a "simple tension" table for hyperelastic material instead of the Mooney Rivlin constants. DesignSTAR seems to use only the Mooney Rivlin constants instead of calculating based on the simple tension table I generate. DesignSTAR seems to delete the "use table" check mark.
I only have simple tension and simple compression data, and Mooney Rivlin constants that are useless since they vary dramatically depending on the range of relative strain.
I have tried using only the "simple tension" table, and have tried using the "simple tension" with the "biaxel tension" tables. P.S.: The simple compression data was used to create the biaxel tension table.
I only have simple tension and simple compression data, and Mooney Rivlin constants that are useless since they vary dramatically depending on the range of relative strain.
I have tried using only the "simple tension" table, and have tried using the "simple tension" with the "biaxel tension" tables. P.S.: The simple compression data was used to create the biaxel tension table.