Simulated PWHT

Status
Not open for further replies.

Quality2479

Materials
Feb 21, 2012
28
What do we mean by Simulated PWHT and where we will be able to find an literature regarding Simulated PWHT. I would like to know this because presently Iam handling an HIC tested plates in which the project specification states that the mechanical tests are to be done after simulated PWHT.
 
Replies continue below

Recommended for you

samples are PWHT just like the part being built

often times hold time for two (2) pwht cycles to cover a repair
 
'Simulated' is probably a poorly chosen word. The test is a simulation, but the PWHT is very real!
 
Status
Not open for further replies.