matschka
Materials
- Apr 23, 2002
- 53
A new QC engineer here has said that the fillet weld on top of a single bevel groove weld specified on the drawing is not necessary because it does not add or increase the strength of the weld joint. He said that the fillet weld is only for cosmetic purposes or to increase fatigue strength.Looking for some technical guidance on this issue.