erosnicolau
Materials
Hi, there,
My question is simple: do I stand any chance of finding some retail (short length) Size 12, Schedule 80, seamless Aluminum pipe anywhere on this planet?
I need it to machine 2 races for a contraption of a large diameter (~300mm), extremely thin bearing-type application, for a slow speed, rarely used gimbal.
Cutting these two rings/races from a solid block is an incredible waste of material and money. Casting is excluded because I need strong aluminum, not the porous disaster yielded by casting. Rolling some flat bar and welding it is the next best thing. Ideally, I could source this kind of pipe, out of which I could machine both races.
Since it's not for an industrial-size project, going to ring-rolling plants is excluded (I guess nobody knows a ring-rolling facility working on retail scale...)
Please, help me out here!
Thank you,
Eros
My question is simple: do I stand any chance of finding some retail (short length) Size 12, Schedule 80, seamless Aluminum pipe anywhere on this planet?
I need it to machine 2 races for a contraption of a large diameter (~300mm), extremely thin bearing-type application, for a slow speed, rarely used gimbal.
Cutting these two rings/races from a solid block is an incredible waste of material and money. Casting is excluded because I need strong aluminum, not the porous disaster yielded by casting. Rolling some flat bar and welding it is the next best thing. Ideally, I could source this kind of pipe, out of which I could machine both races.
Since it's not for an industrial-size project, going to ring-rolling plants is excluded (I guess nobody knows a ring-rolling facility working on retail scale...)
Please, help me out here!
Thank you,
Eros