Apr 13, 2005 #1 mfinke Mechanical Nov 4, 2003 12 0 0 DE Dear all, i´m looking for a SN - curve for the following material: DIN: 0.6035 UNS: F13801 ASTM/AISI: A48, class 55B UK: Grade 350 thank you in advance regards Matthias
Dear all, i´m looking for a SN - curve for the following material: DIN: 0.6035 UNS: F13801 ASTM/AISI: A48, class 55B UK: Grade 350 thank you in advance regards Matthias
Apr 13, 2005 #2 Carburize Materials Sep 23, 2002 702 0 0 US There is a little data in the ASM publication " Atlas of Fatigue Curves" edited by H.E.Boyer - this references "Iron Castings Handbook" edited by C F Walton as the original source for the information. Upvote 0 Downvote
There is a little data in the ASM publication " Atlas of Fatigue Curves" edited by H.E.Boyer - this references "Iron Castings Handbook" edited by C F Walton as the original source for the information.
Apr 13, 2005 #3 metengr Materials Oct 2, 2003 15,478 0 0 US You can also review this thread for additional information on GI castings ; thread330-118025 Upvote 0 Downvote