MrSete

Materials
Dec 9, 2021
1
I need to section some medical PVC tubing (about <5mm of diameter and <1,5mm thickness) to take measurements of its diameter and thickness, in different points of the total lenght. Does anyone have any recomendation on how to do it? I want to distort it the less posible to get an acurate measurement.
 
Replies continue below

Recommended for you

If it were me, I would use some sort of potting compound inside and outside the tube, allow it to harden, and the cut it, and polish the exposed face, and then make the measurement

TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529 Entire Forum list
 