Dec 11, 2004 #1 23513001 Materials Dec 11, 2004 6 US HI, Are their any other solvents apart from Toulene, for Ethylene-Propylene-Diene-Monomer (EPDM). Thanks in advance. Sreedhar.
HI, Are their any other solvents apart from Toulene, for Ethylene-Propylene-Diene-Monomer (EPDM). Thanks in advance. Sreedhar.
Dec 12, 2004 #2 IFRs Petroleum Nov 22, 2002 4,633 US If you go to http://www.coleparmer.com/techinfo/ChemComp.asp, use EPDM for the material and D-Severe Effect for the Compatibility Level, you will find a slew of chemicals that attack EPDM. Perhaps one on this list will help you. Upvote 0 Downvote
If you go to http://www.coleparmer.com/techinfo/ChemComp.asp, use EPDM for the material and D-Severe Effect for the Compatibility Level, you will find a slew of chemicals that attack EPDM. Perhaps one on this list will help you.
Dec 13, 2004 #3 btrueblood Mechanical May 26, 2004 9,844 US Just about any petroleum product (oils, solvents, fuels) will dissolve EPDM. Upvote 0 Downvote