Feb 18, 2002 #1 kiwieng Mechanical Feb 18, 2002 7 0 0 NZ I am trying to coat UHMPE with polycarbonate does anyone know of a solvent that will make this possible
I am trying to coat UHMPE with polycarbonate does anyone know of a solvent that will make this possible
Feb 19, 2002 #2 insideman Mechanical Nov 21, 2000 286 0 0 US There is no solvent for uhmwpe. Upvote 0 Downvote