Hi folks,
We [located in Australia] have a spiral type heat exchanger that has failed in an outer spiral, mostly likely due to fatigue/cold work of the stainless sheet around a row of channel spacer pins. Crack is approx 400mm long, as noted by a fibre borescope visual inspection.
Anyone ever seen a spiral hX repaired before? The vendor has to send someone out from France to effect a repair... only thing is, due to the nature of the spiral hX, we're not sure we've found the only crack! And it's a way complex and involved repair...
Comments, experiences, thoughts?? Can a spiral hX ever be OK in a cyclic service?
Thanks in advance.
Rob
We [located in Australia] have a spiral type heat exchanger that has failed in an outer spiral, mostly likely due to fatigue/cold work of the stainless sheet around a row of channel spacer pins. Crack is approx 400mm long, as noted by a fibre borescope visual inspection.
Anyone ever seen a spiral hX repaired before? The vendor has to send someone out from France to effect a repair... only thing is, due to the nature of the spiral hX, we're not sure we've found the only crack! And it's a way complex and involved repair...
Comments, experiences, thoughts?? Can a spiral hX ever be OK in a cyclic service?
Thanks in advance.
Rob