Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Spline Type Identification

Status
Not open for further replies.

Roncallo

Automotive
Feb 10, 2003
4
I'm trying to figure out How I can identify a spline so that I can have it copied the spline is from an 1986 Mercedes Benz 560SL rear axle shaft. It is most likely a DIN metric spec but I wouldn't know how to measure it accurately. I need to have shorter axle shafts made so I will need the specification of the spline so the machine shop can make it.

John Roncallo

 
Replies continue below

Recommended for you

Splines are measured by go/nogo gages, at least the Ansi ones are. If you know of a shop that makes metric splines, they could probably identify it that way.
 
Not only is that Merc axle spline a metric DIN spline, but it also is likely a 45 deg pressure angle spline. Most production external splines are roll formed (as opposed to shaped) to reduce cost. So a 45 deg pressure angle is used to make roll forming possible.
 