Please provide spot test procedure/solution for detection of trace amounts of hydrogen sulphide on a steel surface and any reference literature in this regard.
 
Replies continue below

Recommended for you

If you want just a qualitative test you can use lead acetate tests strips available at any laboratory supply house.



More meaningful quantitative results can be made using Draeger Tubes.


If you want to have a continuous monitoring system check with your local utility and see which meter they are using.
 