Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

spot welding cooling system

Status
Not open for further replies.

poorjabbar

Mechanical
Dec 17, 2003
1
I want to know more about design & type of cooling systems & its calculating methods usually used in automotive manufacture body shops
 
Replies continue below

Recommended for you

For spot welding application, there are two cooling circuit/requirements you need to calculate.
The first is the cooling for the weld controler. The other is the cooling for weld guns and transformers. your equipment supplier should assist you to decide the requirements of the cooling system. Mostly you need to calculate the GPM requirements. Be careful if the welding is MFDC, the GPM requirement is much higher
 