Has anyone had any experience with Sulphate Reducing Bacterial Corrosssion? We have a ship that has extensive pitting in the ballast tanks on the flat bottom area. How can we nuetralize it? After plate replacement and blasting how would you suggest we treat the minor effected areas after blasting? The classification society has put a condition of class on the vessel to be drydocked in 2 months and we would like to prepare the tanks before then.