Ulther
Chemical
- Jan 15, 2008
- 7
Does anybody experienced severe claus catalyst damage. I am not writing about any deactivation mechanism (e.g. sulfation, sulfur condensation, coke formation, loss of specific area due to hydrothermal conditions)wchich are pretty well described in literature. I am interested in a situation where part of catalyst beads lose their physical integrity and break into pieces. In consequecne large quantity of dust is formed, which cause plugging of pipelines and condensers. Situation leads to pressure drop build up and ultimately to SRU shut down.
What could be a reason for such catalyst destruction (except for high temperature due to sulfur burning during improper unit shut down? Maybe it is worth to mention that this did not happen immediately after catalyst replacement but after a few years of operation.
I would be really grateful for sharing your knowledge. Maybe you had similar problem in your SRU's?
What could be a reason for such catalyst destruction (except for high temperature due to sulfur burning during improper unit shut down? Maybe it is worth to mention that this did not happen immediately after catalyst replacement but after a few years of operation.
I would be really grateful for sharing your knowledge. Maybe you had similar problem in your SRU's?