Can I substitute Black Oxide as a coating for a spec that calls out 304SS?
 
Replies continue below

Recommended for you

Generally a big NO.

Can you come back with more details of the environment the subject will see?
 
pipe, subject to high velocity superheated air, 600+ deg. F
 