I have to run a welding procedure as per Sec IX. MAterial is SS 304 with Solution annealing.Thickness of the coupon will be 1/2" plate. Can someone recommend the solution annealing time and temperature cycle.

Merzi
 
Replies continue below

Recommended for you

Yes. Go to the appropriate ASME Material specification for this grade and look up the minimum solution annealing temperature. The time is based on thickness, typically 1 hour inch, and for thickness less than 1 inch, it will be between 15-45 minutes.
 
Solution annealing to be done at 1035C (1900F) with a rapid quench.

Heating rate as quick as possible, step of 30 minutes at 1035ºC followed of rapid cooling.